BS 8110 limits the depth of lever arm to maximum 0.95 the effective depth. One reason i could find is because the top layer of concrete is usually of poor quality due to bleed water accumulating on top, therefore this limit on lever arm. Still having some doubts. Maybe someone can help
 
Replies continue below

Recommended for you

I seem to remember the la is to the centre of the stress block if it became 1.0 you would have no stress block. There is also some merit in assuming surface concrete may not be as sound as internal material.
 