I recall the 'shenanigans' of the McGuire apartment building in Seattle back in 2010 (Link 1 and Link 2). Summary ==> 9 yo, 25 level PT building that had some strand corrosion issues at tendon ends due to water/moisture penetration from live-end grout pockets...fast forward to 2010/11 and it was demolished! I don't recall if it was discussed here at Eng-Tips at the time.
Well I just read this report Link3 by Bondy, Poston et. al, and whilst the authors do not mention the McGuire building by name (to protect the innocent/guilty?) it is obvious it is indeed the project they refer.
Always interesting in getting the 'other side' of the opinion.
Well I just read this report Link3 by Bondy, Poston et. al, and whilst the authors do not mention the McGuire building by name (to protect the innocent/guilty?) it is obvious it is indeed the project they refer.