We are having really very tough time while producing small metal seated ball valves in the range of 3/4" class 150(Floaters) to 2" class 300(trunnion).we have done all permutation and combination but unable to achieve zero leakage as per API 598.
these valves are for produced water package with a design temperature of 100 deg centigrade max.
even we replaced stellite coating with tunsten carbide coating on ball and seat every efforts is in vain. we disassembled and did some manual lapping that worked a bit on trunnion but floaters are still unresolved mystery.Can some one throw light and provide some useful tips.DM
these are basically carbon steel cast valves with SS trim
these valves are for produced water package with a design temperature of 100 deg centigrade max.
even we replaced stellite coating with tunsten carbide coating on ball and seat every efforts is in vain. we disassembled and did some manual lapping that worked a bit on trunnion but floaters are still unresolved mystery.Can some one throw light and provide some useful tips.DM
these are basically carbon steel cast valves with SS trim