We have a problem in one of our storage floating roof, double deck, tanks. There is a leak from 2 of the pantoon compartments. We measured the oil level inside the leaking compartments and it was 9” and 14” in the two compartments while the floating roof was at 35 feet.
I need your advice on what you think would be th emain cause of this leakage and how to mitigate such a defect. is it also safe to keep the tank in operation in this condition without any risk of the roof.