Recently, I am assigned a project to find reason why our lasor welded part has porosity in the welding bead. Under the microscope, gas bubbles are as large as 5/1000''. The porosity usually exists at the boundary between the bead and the substrate.

As I have little experience with welding porosity anslysis. My questions are: Is there any general reasons that porosity formulate during the welding process? Is there any papers, books devoted specifically to welding porosity?

Thanks in advance
 
What are the materials being joined? How were they fabricated? Are the parts cleaned prior to welding?
 
The material is stainless steel. The substrate surface is milled and grinded. The bead is cold drown stainless steel wire. Surface are all cleaned before welding.
 