bssharpy
Computer
- Aug 7, 2004
- 4
I have just started work at a new company that has recently about six months ago purchased a new MAZAK HYPERGEAR 4 KW laser.
I have worked with two Mazak MKII machines A 2.5 KW and a 4 KW for around 4 years at my previous employer running lights out in an FMS cell.
The HYPERGEAR machine has had a bad history since the installation. The machine only has around 700 HRS on it and it has had the external optics replaced 4 times because of contamination problems. Mazak service is telling me that the external optics are only lasting around 1000 hrs on other installed machines?
Last week Mazak replaced the external optics and we are now getting around 3900 watts at the head. As the optics where contaminated again and we where only getting 1200 watts at the head. With the fresh set of mirrors I have no trouble cutting light gage HRS.
I can cut 0.250 HRS at 100 IPM at 4KW, 0.6KG oxygen, 500HZ, With a 7.5 IN convergence lens at -0.04 focus with a near glass like edge finish. When cutting 0.375 I can get the edge quality acceptable but only at a very slow feed “around 40 to 50 IN a minute at around 3kw.
(Question 1)
Does external optics replacement at 1000 hrs sound normal for a flying optics machine?
(Question 2)
If you have a flying optics machine “TRUMPF, BYSTRONIC, ETC” how long are your external optics lasting?
The MKII machines would go around 4000 hrs or more before optic or resonator service.
(Question 3)
I am trying to cut 0.75 HRS with good edge finish to reduce a machining step. I can get 0.750 to cut but with occasional thermal runaway. I suspect that the thermal runaway is material related as the material is just plain old A36 structural. Any advice as what to look for in thick plate that would attribute laser cutting problems would be helpful. Have you found a specific type of thick plate that cuts well on a laser. Any advise related to cutting A36 thick plate on a laser would be helpful.
I have worked with two Mazak MKII machines A 2.5 KW and a 4 KW for around 4 years at my previous employer running lights out in an FMS cell.
The HYPERGEAR machine has had a bad history since the installation. The machine only has around 700 HRS on it and it has had the external optics replaced 4 times because of contamination problems. Mazak service is telling me that the external optics are only lasting around 1000 hrs on other installed machines?
Last week Mazak replaced the external optics and we are now getting around 3900 watts at the head. As the optics where contaminated again and we where only getting 1200 watts at the head. With the fresh set of mirrors I have no trouble cutting light gage HRS.
I can cut 0.250 HRS at 100 IPM at 4KW, 0.6KG oxygen, 500HZ, With a 7.5 IN convergence lens at -0.04 focus with a near glass like edge finish. When cutting 0.375 I can get the edge quality acceptable but only at a very slow feed “around 40 to 50 IN a minute at around 3kw.
(Question 1)
Does external optics replacement at 1000 hrs sound normal for a flying optics machine?
(Question 2)
If you have a flying optics machine “TRUMPF, BYSTRONIC, ETC” how long are your external optics lasting?
The MKII machines would go around 4000 hrs or more before optic or resonator service.
(Question 3)
I am trying to cut 0.75 HRS with good edge finish to reduce a machining step. I can get 0.750 to cut but with occasional thermal runaway. I suspect that the thermal runaway is material related as the material is just plain old A36 structural. Any advice as what to look for in thick plate that would attribute laser cutting problems would be helpful. Have you found a specific type of thick plate that cuts well on a laser. Any advise related to cutting A36 thick plate on a laser would be helpful.