DOES ANYONE KNOW WHAT THE CUTTING PROGRAM SHOULD BE FOR 24 GAUGE GALVANIZED? IM RUNNING A 1000 WATT MAZAK AND MY CUT SPEED IS 12O IPM AND IM CUTTING AT 600 WATTS BUT IM ENDING UP WITH A ROUGH CUT (BOTTOM SIDE OF PART HAS A BUR ON IT). THE PROGRAM IM RUNNING IS ACTUALLY FOR .035 CRS. I TRIED TO INCREASE AND DECREASE MY SPEED AND PLAYED WITH THE DUTY AND NOTHING SEEMED TO REALLY HELP.
 
NEVERMIND EVERYONE, I WAS CUTTING WITH OXYGEN WHEN I SHOULD'VE BEEN USING NITROGEN. NICE AND CLEAN CUTS NOW
 