Laser Beam Welding technique?

Status
Not open for further replies.

SmithsJohn2

Mechanical
Jun 22, 2005
35
I read a magnazine talking about the new A-380 airbus. They said that laser beam welding technique is used to avoid the need for rivets in A-380. Anyone know this technique? It is a new technology? How long have it been here? What's the difference compared with the traditional welding? Thanks for sharing.
 
Replies continue below

Recommended for you

It's gets a reasonable right up in my 1977 edition of the Sandvik Welding Handbook. In short, this new technology has been around for some time. It's applications are / were for precision welding situations, paarticularly in areas like electronics. At the time they thought it could take over from some applications which were being done by electron beam welding, as there is no requirement for a vacuum.
 
It seems to me that Friction Stir Welding, being a non fusion process, has a much higher potential of being used for aerospace manufacturing than Laser Beam Welding.
See a short notice on AM&P (Advanced Materials and Processes of ASM International) at page 42 in the May 2005 issue.

 