Good Morning to everyone,
I have to check a pressure vessel in 347H material at creep temeperature.
Does someone have Larson-Miller parameters or table for this material?
I have to use it at 1200F.
I want to show that we can use it at 1200F without problem (creep starts from 1050F).


Many thanks
Regards
 
Replies continue below

Recommended for you

API 530. Also data is available in API 579-1/ASME FFS-1.
 