I am looking for a alternate to Aermet 100 for a high speed switched reluctance rotor. M19 lamination is too low in strength Aermet 100 stronger but sacrifices the magnetics.
Maybe there is something in between. Also Carpenter does not make Aermet in .014" thick sheets.
Anyone have ideas?
Maybe there is something in between. Also Carpenter does not make Aermet in .014" thick sheets.
Anyone have ideas?