Do pipe mills that manufacter standard carbon steel pipe, spray the pipe with a lacquer coating before shipping?
 
Replies continue below

Recommended for you

Only if you ask them to.

My motto: Learn something new every day

Also: There's usually a good reason why everyone does it that way
 
Shonuff,

Maybe it's different for different industries, but in the chemical industry, i've never asked for the coating (is it lacquer or enamel?) and have always gotten it.

donf
 
We normally buy from pipe warehouse suppliers. Some of the pipe comes with lacquer - some don't.
 
If it's destined to be"stock" pipe then it's more likely to be coated with some sort of preservative, but large quantities sold to the user probably not unless it's part of the spec.

My motto: Learn something new every day

Also: There's usually a good reason why everyone does it that way
 