kynar tubing

Status
Not open for further replies.

mjbknight

Aerospace
Feb 5, 2003
1
Help! We've applied Kynar shrinkable tubing to some of our sub-assemblies. When it was baked to shrink, the operator had set the oven temp too high. The tubing split. We can't get it off to rework. Tried scraping with a razor blade, but it's not working too well. Is there a method (mechanical, chemical, heat, cold) to remove this more easily?
 
Replies continue below

Recommended for you

Coil winding tapes are formulated to set after exposure to temp. Contact 3M or other mfrs to discuss wrapping your problem and briefly exposing to hot air blower.
 