Are there any safe ceramic fibres out there.
I need to insulate a kiln sidewall that is currently standard insulation brick but didnt want to use ceramic fibre because of the Health and Safety issues.
I managed to get hold of some Ultralite ceramic pellets from a company in Stoke and made some tiles from it. They performed reasonably ok and I can probably get them better still but they wont go over the kiln arch so i might have no choice but use RCFs.
Any advice would be appreciated.
I need to insulate a kiln sidewall that is currently standard insulation brick but didnt want to use ceramic fibre because of the Health and Safety issues.
I managed to get hold of some Ultralite ceramic pellets from a company in Stoke and made some tiles from it. They performed reasonably ok and I can probably get them better still but they wont go over the kiln arch so i might have no choice but use RCFs.
Any advice would be appreciated.