Jointing chemical for PVC film/sheet to be layed in reservoir

Status
Not open for further replies.

imtiyaz

Mechanical
Jan 4, 2001
29
hi,
I am looking for a jointing chemical/glue for joining PVC sheet(thk of 1mm)which will be laid in raw water reservoir of water head of 8 mtrs.
this sheet will be covered by sand and then castinsitu concrete slabs.

Regards,
imtiyaz

Takecare
Take care
 
Replies continue below

Recommended for you

Try methylene chloride, it will perform a cold welding together of the pvc by a slight disolving and then drying out. The two sides must be very clean - like brand new. Otherwise, try PVC piping cleaner and glue - they work great and are used for water piping. You should be able to find a bulk supplier. This assumes you have gotten no support from your PVC sheet supplier - go up the ladder of distribution and get to the manufacturer of the sheet, too.
 