Is JIS H3250 brass the same as C2600 or C26000 brass. I have some terminals mfg overseas and first they tell me that C2600 is the same as C26000, but then also reference the JIS H3250 as material used.
What gives?
 
JIS H3250 is a standard for copper & copper alloy rods and bars which then references a number of different grades (chemical composition, properties, etc.) such as C 2600. In North America, ASTM B927/927M is the standard for brass rod, bars and shapes, and UNS C26000 is one of the grades referenced therein.
 