Japanese surface texture interpretation? 2

Status
Not open for further replies.

Ceramicguy

Materials
Mar 28, 1999
104
I have a Japanese drawing (I think) with a surface texture callout I don't understand. The symbol looks like a standard surface texture symbol allowing for material removal but has a alphanumeric code above the closed triangle of either 3S or 18S. Any ideas on a conversion to an Ra, Rz, Rt or similar? See the attachment for clarification of my description.

Bruce
 
Replies continue below

Recommended for you

That is an old designation system from previous versions of JIS B 0601. It is indicating Rmax in micrometers.
 