ISO steel standard

Status
Not open for further replies.

aptaed

Materials
Aug 18, 2006
2
HI! Where I can find ISO metal designation? For example: EN24T what the type of steel is this,and so on. I need it for speeds and feeds calculations for CNC. I've tried to find it but found nothing. Thank you very much in advance.

 
Replies continue below

Recommended for you

EN is a British designation. I found info on EN steels by searching on UK based search engines. Use google.co.uk, yahoo.co.uk etc., instead of .com
 
EN24 is a very old designation, in BS 970 (1955)
= 817M40 in BS 970 (1991).
"A nickel chromium molybdenum steel with high strength and toughness. Used for gears axles and high strength studs. Supplied as rolled, annealed and hardened and tempered. Supplied as black round or square bar and bright round or square, and hexagons." --
A suffix T = supplied in the hardened and tempered condition.
For composition, see
The US equivalent is 4340. From the international alloy crosslisting for 817M40 at
 
Thank you very much for advice,I'll try all links.The very first link I've tryed already but the problem is that I need to pay to get rights to look at it,at the moment it impossible for me... :)
 