Is there a book (or two) that contains all the ISO rubber test methods?

I'm based in the US and have the two ASTM books that give all the test methods (for tensile, tear, abrasion resistance, etc.), but sometimes get specs from customers that reference ISO test methods, so I'd like to get copies of these methods. It'd be convenient, obviously, if there was a book or two that I could get that would have this info, rather than purchasing all the specs individually.

Thanks,


Tom Jablonowski, TSE Industries, Inc.
 
Replies continue below

Recommended for you

ISO standards are published individually and not as collections in book form like the ASTM specs - sorry Tom.
 