ISO Codes 1

Status
Not open for further replies.

Vestveit

Materials
Sep 13, 2008
5
Hello,

How common are the ISO welding codes in the U.S? Most of the Q & A's here seems to be related to ASME or AWS in one way or the other.

A welding company delivering goods to the offshore sector in Europe will normally be required to be certified according to ISO 9001 & ISO 3834-2, how common is this in the U.S.?

Also, are welding engineers required to be certified under the American codes? Normally ISO codes will call for a qualification at international level (IWE, IWT or IWS) or an acceptable national equivalent.
 
Replies continue below

Recommended for you

ISO 9001 only qualifies the Quality Management System of the company, not the quality of the welding.

Ted
 
ISO 3834-2:2005 Quality requirements for fusion welding of metallic materials -- Part 2: Comprehensive quality requirements
 