I have a hemispherical head with a cast nipple 1.25" in diameter and 1.50" long. The first .75" of the nipple is threaded with a 1.25" thread. The remaining .75" of length is straight 1.25" OD.

I was told that the straight OD on the nipple needs to be 1.38" OD and the length of the straight OD needs to be at least 1" long. I inquired as to why, and I was told that there is a minimum requirement in ASME in regards to this.

Could someone possibly quote me the paragraph in section UW-16 that would apply to this instance?? I don't believe ASME has minimum requirements on nozzles or openings until you reach 3" in diameter.
 
Replies continue below

Recommended for you

Cast Nipple?

Need more info. and talk to your AIA....change coming to UW-16.
 
BOP..

Wow.... what materials are used in the head and nipple ?

Is this cast iron ?

-MJC

 
After some searching, the only thing I can come up with is that he is mistaking it for a flued opening. But it clearly states that there is no minimum requirements for a flued out opening under 6" in diameter.

BTW, yes it is a cast nipple. The "vessel" is actually a pulsation dampener that is only about 15" OD. But it operates at a constant 2000psi, so it is a pressure vessel. We cast it out of SA-352-LCB material (17,500psi min. yield.)

The real reason I am inquiring about this is that the "engineer" in charge was about halfway through this project and was using a non-coded material. Castings made and material being poured. Personally, I don't think this guy knows his a$$hole from his earhole.
 
The real reason I am inquiring about this is that the "engineer" in charge was about halfway through this project and was using a non-coded material. Castings made and material being poured. Personally, I don't think this guy knows his a$$hole from his earhole.