Eng-Tips is the largest forum for Engineering Professionals on the Internet.

Members share and learn making Eng-Tips Forums the best source of engineering information on the Internet!

  • Congratulations dmapguru on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Is there anyway to prove equivalence of different material from different codes ?

Status
Not open for further replies.

hamidinho

Petroleum
Joined
Nov 29, 2022
Messages
20
Location
DZ
Hello guys,

So i've got an issue with a project, we need to find an equivalent to a material from a french code which is TU37C, because it's unavailable in the market -we have only astm material-. I've done some researches and i've found out that likes of A106 Gr A, A192.. are equivalent but the issue is that its mentioned in a table on different websites and without any codes that state that these are equivalent. So i'm asking how would you guys prove it to the client ? or if there's some code that states equivalent material from different codes (like french and american or european and american)

Thank you,
 
Get a copy of the ASTM document that covers the material and whatever document covers TU37C and compare them.

They will no doubt be different in some aspects, so what one really requires are the minimum properties required for the task.

If one is X tensile yield and the other is Y tensile yield and both of them exceed the required tensile yield (and factor of safety, et al,) then you are good to go.

 
Thanks guys your help is much appreciated.
 