I am looking for the ASTM standard D3039 and D3158, both for plastic,
I think it should be somewhere in Vol: 08.02, but I just can not find it right now, I will use it in urgent.

If any of you have this standard, pls send it to me.

Xinrongding@hotmail.com

Thank you.
 
ASTM D 3039/D 3039M Standard Test Method for Tensile Properties of Polymer Matrix Composite Materials

is in volume 15.03, or available at:


ASTM D 3158-83 Specification for Asphalt Saturated and Coated Organic Felt Used in Roofing was withdrawn in 1983.

Regards,

Cory

Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
 
I found a problem, because I need dogbone samples for +45,-45 Twintex, what is the standard for dogbone specimen?
 