Ontario Provincial Standard says that you should check the hydrometer dimensions (L1, L2, Vb, A) yourself, because the ASTM does not specify the dimensions.
I have found that universally used dimensions (L1=10.5, L2=14, Vb=67) are different from what I measured. especially the Vb ( Volume of Bulb). The universally used is 67cm3 and my measurement is 57-60cm3 although this difference does not affect the final result significantly.
Any comment on this? Thank
I have found that universally used dimensions (L1=10.5, L2=14, Vb=67) are different from what I measured. especially the Vb ( Volume of Bulb). The universally used is 67cm3 and my measurement is 57-60cm3 although this difference does not affect the final result significantly.
Any comment on this? Thank