I have a Stainless Steel 304 butt welded (SAW) with a MDMT of -196°C.
The base metal and HAZ are exempt from impact testing per UHA-51(d)(1)(a).
The weld metal is not exempt from impact testing per UHA-51(e). The PQR therefore has impact testing.
For the minimum coupon thickness, QW-403.6 (minimum base metal thickness when impacted testing is required) supplementary essential variable is contained within the base metal section (QW-403). A vendor is claiming that QW-403.6 only applies if the base metal requires impact testing and that if only the 'weld metal' requires impact testing then this supplementary essential variable QW-403.6 does not apply.
Where does is specify that if any zone (base, HAZ & Weld) needs impact testing than QW-403.6 applies? QW-251.2 gets close. however only mentions materials rather than zones.
The base metal and HAZ are exempt from impact testing per UHA-51(d)(1)(a).
The weld metal is not exempt from impact testing per UHA-51(e). The PQR therefore has impact testing.
For the minimum coupon thickness, QW-403.6 (minimum base metal thickness when impacted testing is required) supplementary essential variable is contained within the base metal section (QW-403). A vendor is claiming that QW-403.6 only applies if the base metal requires impact testing and that if only the 'weld metal' requires impact testing then this supplementary essential variable QW-403.6 does not apply.
Where does is specify that if any zone (base, HAZ & Weld) needs impact testing than QW-403.6 applies? QW-251.2 gets close. however only mentions materials rather than zones.