is it possible to use SA105 material for tube sheet in shell & tube heat exchanger ? 1

Status
Not open for further replies.

gh61

Mechanical
May 25, 2016
15
is it possible to use SA105 material for tube sheet in shell & tube heat exchanger ?
thaks a lot
 
Replies continue below

Recommended for you

gh61, welcome to Eng-Tips. Please note that it is considered "bad form" to double post. Please consider "red-flagging" (Report) this post and asking that it be removed. The discussion can then continue in the ASME forum. Thanks in advance

The problem with sloppy work is that the supply FAR EXCEEDS the demand
 
as per clause 1 (scope) of SA 105, Tube sheets are not included within the scope of SA 105 Specification.
 
What is the Code of construction?

The problem with sloppy work is that the supply FAR EXCEEDS the demand
 