Eng-Tips is the largest forum for Engineering Professionals on the Internet.

Members share and learn making Eng-Tips Forums the best source of engineering information on the Internet!

  • Congratulations dmapguru on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Is it possible to implement non-linear thickness modulus with Continuum shells?

Status
Not open for further replies.

at13987

Mechanical
Joined
Apr 21, 2016
Messages
1
Location
GB
Hello,

I have developed a hypoelastic VUMAT which describes the behaviour of woven fabrics during forming processes for composite manufacture. The VUMAT works fine, however I need to enhance the model by considering the through thickness compliance of the fabric. To do this I have been considering using Continuum shell elements (SC8R).

When using these elements I have to define a Thickness modulus. As the compressive stiffness of the fabric is non linear, I would like to update the modulus incrementally based on the strain.

I believe the material definition for this element remains plane stress and so I don't believe I can do this directly using my VUMAT, therefore I need a work around. Does anyone have any suggestions for this?


Thanks

AD
 