my question today is if HIC test (as described in NACE 284) is applicable for low alloy CrMo steel plates and for Pressure vessels in wet H2S service. Or is it only applicable for Carbon steel (C-Mn) plates? What about fittings?

Thanks!
 
Replies continue below

Recommended for you

Yes, it applicable to Cr-Mo steels. It is applicable to any kind of part.
 