When raising the pH of ground water with high fe2+ concentration of 47ppm, using NaOH or Lime, a green floc is produced - if the water is aerated first, the floc is brown?
Both situations result in iron removal but I am curoius as to what is actually happening?
Regards
Both situations result in iron removal but I am curoius as to what is actually happening?