My customer references ASTM A747 Gr. CB7Cu-1 in their material spec. Parts are required to be HT'd to the dbl H1150 condition. I accompany each lot of castings with a set of 4 test pins (3 1/2" long, threaded on both ends...).
I've been having a problem lately getting the yield strength to pass. My minimum req'ts are as follows:
UT - 125K, Y - 100K; Elong 15%, RA 35%. My results for yield has been in the 90-98K range and tensiles sometimes hover near the minimums as well.
Castings and pins are first solution annealed at 1900F as per the spec. We've even experimented with the H1150 M alternative, which is allowed by our customer. This is where the first age is at 1400F for 2 hours followed by an 1150F for 4.
Any ideas or new resources would be helpful.
I've been having a problem lately getting the yield strength to pass. My minimum req'ts are as follows:
UT - 125K, Y - 100K; Elong 15%, RA 35%. My results for yield has been in the 90-98K range and tensiles sometimes hover near the minimums as well.
Castings and pins are first solution annealed at 1900F as per the spec. We've even experimented with the H1150 M alternative, which is allowed by our customer. This is where the first age is at 1400F for 2 hours followed by an 1150F for 4.
Any ideas or new resources would be helpful.