go to your machinery's handbook and use existing formulae for determining whatever dimensions you need.
 
Internal Pd. 3.8607-3.8547
major Min. 3.8750
Minor 3.849-3.841
External Pd. 3.8533-3.8487
Major 3.8736-3.8677
Minor 3.8398-3.8284