I started to design a new stud and picked a thread out of our standards book that has an oversize pitch diameter. I don't know if it was designed to any kind of standard, although sometimes a Class 4 is mentioned.
Then I looked at the Class 5 threads in Machinery's Handbook. The question I have is do you have to apply Class 5 to both internal and external, or can you have Class 5 on the stud and Class 2 or 3 in the tapped hole?
I understand that you can check the stud threads by pitch diameter, but you need a gage for the tapped hole. Our shop is not going to be willing to buy more thread gages, so I might have to resort to using our old standard and be done with it.
Thanks for any enlightenment.
Then I looked at the Class 5 threads in Machinery's Handbook. The question I have is do you have to apply Class 5 to both internal and external, or can you have Class 5 on the stud and Class 2 or 3 in the tapped hole?
I understand that you can check the stud threads by pitch diameter, but you need a gage for the tapped hole. Our shop is not going to be willing to buy more thread gages, so I might have to resort to using our old standard and be done with it.
Thanks for any enlightenment.