Inspecting galvanization

Status
Not open for further replies.

corrosion10

Civil/Environmental
Oct 24, 2010
9
White corrosion products are observed on the galvanized steel piles within a month, some minor and some more severe. The client shared some photos of the piles. The surface looks uneven, and some spots are not coated or the coating peeled off. Is there any protocol for inspecting the galvanization other than measuring the thicknesses? My assessment is the storage condition may have contributed to the white storage stains, but I am afraid the quality of the galvanization may also play a role. I am not sure how to prove or disprove the galvanization quality though. Any insight is appreciated.

4_afqr9r.jpg
1_rccf1g.jpg
7_kk2kv8.jpg
2_muwnca.jpg
3_ykj6j4.jpg
5_o4jdbi.jpg
6_yfc5ec.jpg
 
Replies continue below

Recommended for you

Consider also contamination from carbon steel which can be in close proximity, used for handling etc.

Per ISO-4126, only the term Safety Valve is used regardless of application or design.
 
Visit the American Galvanizing Association website. They provide a good deal of information on the subject of "how to" galvanize properly, i.e., from the design stage to preparing the material for galvanizing to inspection of galvanized material.


Best regards - Al
 