Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations TugboatEng on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Induction motor frame 1

Status
Not open for further replies.

PAP

Electrical
Joined
Jul 7, 2002
Messages
37
Location
TH
Dear sir
Anyone can help me about the standards of the frame of motor.
Thank you.
 
fractional horsepower motors use 2-digit frame designations, integral use 3-digit frames.
First 2 digits always shaft height in inches times 16 (small machines) or times 4 (larger machines).

For example, frame 48 has 3” shaft height.

445 has shaft height of 11”.

The 5 at the end of 445 can be used to determine length by table lookup. Many more dimensions are defined which help to ensure mechanical interchangeability of motors.
 