Can anyone tell me about the bolts PN 84779-20. I found in the outboard stabilizer to constant section attachments. At this time, these bolts should be from Inconel, but I am not sure. Please help me to find the specifications of these bolts.
 
Replies continue below

Recommended for you

A quick google search of 84779-20 turned up some results.

You might want to state what aircraft etc. they are used on to get a more complete answer.

Posting guidelines faq731-376 (probably not aimed specifically at you)
What is Engineering anyway: faq1088-1484
 
These bolts are installed in the aircraft DC10-30F. They are located in the attachments of the outboard horizontal stabilizer with their constant section of the stabilizer. All that I found in google was, where can I buy them. But the specifications or material type, did not find.
 
Contact FIT Technologies ( or send me an email (robert.farhat@bdk.com) with details of what you are seeking and I can forward to proper contact. FIT specialize in NAS bolts as well as exotic bolt materials.
 