Jul 20, 2012 #1 Kenny1130 Industrial Joined Jul 12, 2012 Messages 12 I am cutting Inconel 625 O.D. 9.75. I have 94 cuts to make. I am out of Carbide so that leaves with bi metal. The blade although bi metal it is a very aggressive bi metal. Any suggestions on feeds and speeds.
I am cutting Inconel 625 O.D. 9.75. I have 94 cuts to make. I am out of Carbide so that leaves with bi metal. The blade although bi metal it is a very aggressive bi metal. Any suggestions on feeds and speeds.
Jul 23, 2012 #2 TVP Materials Joined Apr 12, 2002 Messages 4,592 Location US Table 14 in this publication from Special Metals has data on band sawing various nickel alloys using bi-metal blades: http://www.specialmetalswelding.com/publica/Mach.pdf Upvote 0 Downvote
Table 14 in this publication from Special Metals has data on band sawing various nickel alloys using bi-metal blades: http://www.specialmetalswelding.com/publica/Mach.pdf
Jul 24, 2012 Thread starter #3 Kenny1130 Industrial Joined Jul 12, 2012 Messages 12 Thanks for the info. Upvote 0 Downvote