Does anyone know a supplier of incolloy 800H tubes (10"x12.7mm - seamless)? Any info much appreciated.
 
Replies continue below

Recommended for you

try the trade name for inconel alloys who owns the name,
so they will know who they licence it to.
er
 
Seamless alloy 800H pipes are to my knowledge only available up to 8 inch. Above 8 they are welded.
 
thank you to all, guys. It seems that ijzer is right about the max dimensions. Nevertheless, I am astonished by this imperative request for seamless tube. As long as a welded tube would be manufactured in strict accordance to ASME rules, I don't see any problem. Any ideas?
 
Just for info: TPS Technitube seems to be able to supply it
 