Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations TugboatEng on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

impact results - UHT material´s welding 1

Status
Not open for further replies.

FernandoL

Industrial
Joined
Jun 29, 2016
Messages
9
Location
DE
Dear colleagues,

I hope this message finds all you well

Project: ASME VIII- Pressure vessel - material ASME SA517 Gr B. Thickness 9,5 mm.

I have to qualify a WPS for welding ASME SA517 - B with impact requirements at -40 C,

Also is required PWHT, and my first results of impact test @-40C of test plate were very low. (lateral expansion less than 0,2mm and energy less than 20J)

The declared Values of certificate of consumable is 75J @ -73C !!!

Can the presence of PWHT changes so much the values of impact? (certificate´s value is "as welded" and my results is "after PWHT".

Any help will be very useful.

Thanks a lot,

Fernando Lescovar Neto
 
Most certainly PWHT can effect impact behavior of weldments. Exposure to elevated temperature from PWHT can result in secondary hardening for some alloys, thus lowering the impact values from as-welded values.
 