Hello All,
I am trying to calculate the energy absorption of lexan and 1010 steel. I know that this value is equal to the area under the stress-strain curve of each of the materials, but I am having trouble finding the stress-strain curve for lexan. Does anyone have this information? or can point me in a direction?..Thanks!!
I am trying to calculate the energy absorption of lexan and 1010 steel. I know that this value is equal to the area under the stress-strain curve of each of the materials, but I am having trouble finding the stress-strain curve for lexan. Does anyone have this information? or can point me in a direction?..Thanks!!