Dose anyobe have advice on how to produce IGA / IGO on 8740 and A286 samples. This is for round-robin testing to fulfill NADCAP requirements. Basically, I am trying to determine how to cause the condition to produce test samples.
 
Replies continue below

Recommended for you

Allow oxygen into the furnace during elevated temperature processing.
 