I have been searching for a definitive listing of %IACS (International Annealed Copper Standard) values. I found a lot of online sources that had varying levels of information, but no single listing that seemed to cover the entire spectrum - and most were very poor with referencing their source material. I'm hoping some of you may know a good reference that is well documented - or where I can get my hands on the standards themselves. Please don't limit yourselves to online info, I'd be happy to pay for a good book or reference.
Here is an example where this was needed. Two 2024-T62 panels were briefly exposed to extreme temperature exaust. The technical data called out for NDI to perform electrical conductivity checks of the material to ensure that the material properties of the effected areas have not been compromised. I found several sources for %IAC range for 2024-T62 Aluminum, but none that in turn listed their source of that information.
So - if any of you have "been there done that", I'd appreciate not having to dig around any more than I have to...
Thanks in advance...
Here is an example where this was needed. Two 2024-T62 panels were briefly exposed to extreme temperature exaust. The technical data called out for NDI to perform electrical conductivity checks of the material to ensure that the material properties of the effected areas have not been compromised. I found several sources for %IAC range for 2024-T62 Aluminum, but none that in turn listed their source of that information.
So - if any of you have "been there done that", I'd appreciate not having to dig around any more than I have to...
Thanks in advance...