I am looking for the procedure for hardfacing the drum safety valve seat (operating temp ~ 400 C) but i don't know what number of stellite for this safety valve if material of seat bushing is SA 182 F347

I would appreciate any suggestions for this answer.
 
Is this a Crosby Valve?
#6 Stellite with Standard Overlay
MInimal Preheat, No PWHT
Gas Tungsten Ara Welding (TIG) Procedure

J. Alton Cox
President
DeLuca Test Equipment
 
Thank you for your suggestion .My safety valve is consolidated type 1700-S2 if you have any more information please recommend me again
 
Since the loading on the Valve seat in a Safety Valve is of Impact nature and Stellite is poor in withstanding Impact loads, generally Stelliting of Seats of a Safety Valve is not recommended.
 
About Stellite, you can also see:
Thread725-23517 ;
Thread330-23518 .
Maybe you'll find some useful links...