Hydrostatic test of A106 Gr.B Pipes

Status
Not open for further replies.

mhat

Materials
Joined
May 19, 2006
Messages
4
Location
TR
During the hydrostatic testing of A106 Gr.B pipes, is it possible to check along the length of the pipe during hydrostatic testing or some portion from the ends can not be tested due to plug insertion etc.?
Thank you.
 
Pipe may be hydrostatic tested in the factory by the manufacturer. Purchaser may possibly specify factory NDE in lieu of hydrostatic test or neither. Inspection test pressures produce a stress in the pipe wall equal to 60% of specified minimum yield strength (SMYS) at room temperature. Pressure is maintained for not less than 5 seconds. Monitoring of the hydrostatic testing is accomplished by observation of the pressure.

The piping code sets the requirements for hydrostatic testing in the field.

What are you trying to accomplish?
 
Are you talking about a mill test?

They are pretty brutal but normally they don't use internal plugs for that very reason, but press seals at the end. You normally only get 10 seconds or less per test so no you don't see much and there is water everywhere.

Is that what you mean?

Remember - More details = better answers
Also: If you get a response it's polite to respond to it.
 
Thank you for your interest. I am looking for the mill hydrostatic test.
Let me repeat the question; during the hydrostatic testing of A106 Gr.B pipes at mill, is it possible to check along the length of the pipe?
 
Yes, but you don't get very long - 5 to 10 secs max and there is a LOT of water flowing about.

You often don't get good access all the way around. Some mills do it vertically so unless you're 12m tall you won't see anything.

What exactly are you trying to achieve?

see this e.g.

Remember - More details = better answers
Also: If you get a response it's polite to respond to it.
 