I found this helpfull forum during my
I am a enigneer for rubber compounding in Germany.
I have to develop a white EPDM compound for food contact.
My problem is to find a silica filler, that is hydrphob, this means treated with silan by the producer,
or a single silane (to mix it together with untreated silica in our internal mixer)
that complies with FDA 21 CFR 177.2600.
This is because of the parts should have a low water swelling and good abrasion resistance.
Or are there any other opportunities.
Uwe from Germany
I found this helpfull forum during my
I am a enigneer for rubber compounding in Germany.
I have to develop a white EPDM compound for food contact.
My problem is to find a silica filler, that is hydrphob, this means treated with silan by the producer,
or a single silane (to mix it together with untreated silica in our internal mixer)
that complies with FDA 21 CFR 177.2600.
This is because of the parts should have a low water swelling and good abrasion resistance.
Or are there any other opportunities.
Uwe from Germany