Hydra-lock Conform-A chucks...does anybody have any experience with them?
I'm working on a problem part right now. Ø105.3 mm flange OD, Ø96.015 mm minor OD, and a thru hole of Ø78.7 approximately. The part is roughly 16.5 mm long with a 6.35 mm thick flange. The material is 303 stainless.
Coming to my machining center, I've got pre-molded parts that are out of round up to about 0.008" (0.203 mm), and the out-of-roundness varies across all three diameters. Since I turn every surface on the part, the operation is done in two steps in a twin spindle lathe. My problem is the Ø96 feature. I have a total tolerance of 0.03 mm and a total roundness spec of 0.03 mm.
I've used various combinations of pie jaws and pressures, both ID and OD, to try and get the parts round, but I'm still intermittently running into tri-lobe forms and egg-shapes that take me out of spec. I can make parts to print, but with 100% inspection end up with about 40% fallout. I can add a third operation that clamps just the faces of the part and trues up the flange Ø 1st. Then my normal machining process takes over. I end up with a round part but have an added operation.
I've gotten mixed reviews on the Hydra-lock Conform-A chucks that say they can conform to the part ID or OD without rounding it up (up to 70% that is). Based on their calculations, two of these chucks in sequence will solve my issue. Has anybody on the boards used these chucks in production machining? Pros? Cons? Have you used any other workholding styles for a similar issue?
My added 3rd step makes the parts to print, but needless to say mgmt doesn't like the added cost. I've thought also about an expanding collet with a high number of "fingers", but I think the pressure may still be enough to deform the part.
Thanks in advance!
I'm working on a problem part right now. Ø105.3 mm flange OD, Ø96.015 mm minor OD, and a thru hole of Ø78.7 approximately. The part is roughly 16.5 mm long with a 6.35 mm thick flange. The material is 303 stainless.
Coming to my machining center, I've got pre-molded parts that are out of round up to about 0.008" (0.203 mm), and the out-of-roundness varies across all three diameters. Since I turn every surface on the part, the operation is done in two steps in a twin spindle lathe. My problem is the Ø96 feature. I have a total tolerance of 0.03 mm and a total roundness spec of 0.03 mm.
I've used various combinations of pie jaws and pressures, both ID and OD, to try and get the parts round, but I'm still intermittently running into tri-lobe forms and egg-shapes that take me out of spec. I can make parts to print, but with 100% inspection end up with about 40% fallout. I can add a third operation that clamps just the faces of the part and trues up the flange Ø 1st. Then my normal machining process takes over. I end up with a round part but have an added operation.
I've gotten mixed reviews on the Hydra-lock Conform-A chucks that say they can conform to the part ID or OD without rounding it up (up to 70% that is). Based on their calculations, two of these chucks in sequence will solve my issue. Has anybody on the boards used these chucks in production machining? Pros? Cons? Have you used any other workholding styles for a similar issue?
My added 3rd step makes the parts to print, but needless to say mgmt doesn't like the added cost. I've thought also about an expanding collet with a high number of "fingers", but I think the pressure may still be enough to deform the part.
Thanks in advance!