HY80 2

Status
Not open for further replies.

3lilaggies

Mechanical
May 4, 2006
52
Looking for specs on HY80 perferably MIL, but will take anything. Looking to qualify a procdure. MIL spec givin is MIL-S-2300BC can't find anywhere.
 
Replies continue below

Recommended for you

Are you sure that the MIL spec is not MIL-S-23008C or 9C? Both deal with HY80 forgings, but have been canceled. Try checking for MIL specs at


The MIL standards that deal with welding of HY80 are MIL-STD-1689 for surface ships, and MIL-STD-1688 for submarines (although 1688 has been replaced be a Techincal Manual for a lot of applications)
 