Hi all.
We have a problem in our Huck 256 tool. The Huck bolt is getting broken after triggering the Huck gun. But the Huck gun is getting stuck in the bolt itself. We could not remove the Huck gun with ease as usual. We have tried recharging the Huck gun with proper recommended oil. But the problem still exists. Kindly share your ideas to resolve this problem. Thanks in advance.
 