HTV silicone rubber for surge arresters

Status
Not open for further replies.

Makswell

Chemical
Jan 24, 2021
1
Hi,

Can anyone help me with compounding silicone rubber for high voltage applications? Like arresters and cut-out fuses

I need to know what are useful level of ATH loading and how to compensate for poor mechanical properties due to high filler loading?

 
Replies continue below

Recommended for you

I expect that ATH (alumina tri-hydrate) will greatly improve structural properties of HTV (high temperature vulcanizing) silicone. It will increase the hardness and modulus. I would start with a 50% by weight loading. The surface hydroxyl groups in ATH reacts with RTV (room temperature vulcanizing) silicone like moisture and will cause it to cure in minutes. The result is a material that bounces like a superball.

Here is a top Google hit:
 