Hi,

I am working on a program that has run in to difficulties. We have had to revert to an earlier design which used a certain epoxy mix that is now obsolete. Because I work in the Space business we have to use the same epoxy that the design was qualified with. If anyone has any HT972 Hardener in their stores that they would be willing to part with I would be really interested.

Here's hoping I find a needle in a haystack!

Regards,

John Shiell
 
JPS25061971 (Aerospace)
Try moving this post to the composite engineering group forum 327.
You may get a better response there. I am presuming you have already talked to Ciba.
B.E.
 
That product is probably owned by Huntsman now but their website is very difficult to navigate. Huntsman just got bought out but I don't think this has changed their website yet.
 