Howdy all,
I'm trying to figure out how to callout this marking process, since nothing in AS478 seems to cover it. We want to mark a part using a laser to cure a coating onto stainless steel sheet. The process is to apply dry moly lube or a specialty product like CerMark and then cure the material using a ~60W CO2 laser similar to what Omtech makes. After cure the part is cleaned and the un-cured coating wipes away leaving a clear dark mark. For my limited testing the marking seems stable and solvent/skydrol resistant.
Thanks,
-Kirby
I'm trying to figure out how to callout this marking process, since nothing in AS478 seems to cover it. We want to mark a part using a laser to cure a coating onto stainless steel sheet. The process is to apply dry moly lube or a specialty product like CerMark and then cure the material using a ~60W CO2 laser similar to what Omtech makes. After cure the part is cleaned and the un-cured coating wipes away leaving a clear dark mark. For my limited testing the marking seems stable and solvent/skydrol resistant.
Thanks,
-Kirby