I am running a test to see if polycarbonte and polysulphone can withstand oil we are using at 120C. To do this I have the test peices in a large 1.5-2 gallon glass jar. Does anyone have any idea what kind of heater I can use to heat the oil up to and keep it at 120C for days? It needs to be a relatively inexpensive and safe heater.
I would use a fish tank heater but they do not get near those temps.
 
Replies continue below

Recommended for you

A hot plate and combination of cheap single channel process controller and a thermocouple. Might need a relay depending on the controller's switching capacity.
 
The Corning Stirrer/Hotplates can achieve a steady 120 deg C. It's a Rheostat, so you need to calibrated the knob (1-10) to actual temperature, and just leave it there. I've had good luck with them. They're about $300.

ChemE, M.E. EIT
"The only constant in life is change." -Bruce Lee
 